A while back somebody posted a photo of a pot with a white matt glaze with a light green glaze over it  The white matt had rutile in it & was very nice layered under other glazes.  Several of us asked about the recipe.  It was given  I mixed up a 100 gram test batch & did several tests under a lot of different glazes, most of which came out very nice.  It is time to mix up a larger batch & I cannot find the recipe, nor can I find it here on the forum, not even the picture!!  I know I did not dream this all up, `cause I found the almost empty test bottle last night while looking for another glaze.  Somebody help me please, before I go crazy(all this heat doesn't help either!)  Thanks,  Jeff

Views: 223

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Donna Ferrara on July 1, 2012 at 6:14pm

no prob, i know the feeling--especially when it's related  to my glasses or car keys!  can't wait to see your results

Comment by Jeff Poulter on July 1, 2012 at 12:01pm

Thanks girls!

     You have saved my sanity!  I had looked & looked.  I had even gone through every picture posted, but I guess it doesn't pull up the ones in a blog.  I'm glad I have this & can now mix up a real batch  It's always good to know there is at least a little sanity in your life.  It is so hot out that I only fire at night now & of course have a muffin fan sitting on top of the control panel.  jhp

Comment by Donna Ferrara on July 1, 2012 at 6:14am

hi Jeff

I had posted this glaze and a picture of 2 mugs. on both mugs the overall glaze was this matte white, and the rim dip was the copper matt. One mug was sprayed with a wash of lith carb and strontitum....then Jan did the tests of this white too.....hope this helps!  I think the original picture of the mugs is on my photo stream

 

matte white

Cornwall stone        21%

Ferro 3134              22%

Dolomite                21%

Om4 Ball Clay         15%

Flint                       20%

_______________________

                            99%

bentonite                  2%

this is a flat matte white glaze, smooth surface,my experience has been firing it from cone 5-6 1/2 with good results

for colors add

.50% periwinkle blue

4% rutile for a semi matte white, that breaks over dark clay nicely

4% CuCO3 for a copper matte

3% RIO, 1.75% CuCO3, .375% magansese dioxide, .50% rutile for a mustardly brown green

Comment by Jan Wallace on July 1, 2012 at 12:50am

Hi Jeff, Is is with respect to the photo in the link below?

http://cone6pots.ning.com/photo/tabletop?xg_source=activity&xgi...

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service