What is your experience with ceramics in general. (Long answer encouraged)
I starting working in clay about 23 years ago. I wanted to pursue a creative activity besides my full time job. I maintained a studio and sold my pots at studio sales over the years. Two years ago I retired from my full-time job of 27 years, never looked back, and stepped into my studio full time.

I work with Miller clay, stoneware, cone 6 electric. I've experimented with down firing and also agree that a Ramp of 50 degrees does give the best results for most of my glazes.

I'm always searching and experimenting to find new glazes and to add interest and movement to the surfaces. I tend to like a satin finish.

Right now I'm toying with the idea to change over to a porcelain clay. This of course will change everything which I welcome. I have to use the remaining brown stoneware and then begin the clean-up of my studio. This is quite a step and makes me pause. I have worked in porcelain in the past so I do know what I'm getting into.
What is your current involvement with electric fired ceramics? (long answer encouraged)
As mentioned I am currently a functional potter. I do have a group of glazes that are reliable and that I like very much.

I do still test for new glazes. I feel like I'd like to enhance the surfaces of my pots - whether with new glazes or texture so I do experiment.
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
I thought it would be a good idea to communicate with others and exchange ideas. There are not too many functional potters in my area. I do not belong to a co-op or guild because they are all quite a distance from my location.

I'm hoping this forum will be a place where there can be a change of ideas. Also to exchange results and frustrations of testing.

I saw the result of the White Bird glaze which I like. I'm hoping I can get the recipe.
Where do you work on your ceramics projects?
home studio
Do you have your own, or participate in other ceramics Websites:
http://potsbyliz.comp
How did you find this network?
Link or reference from another site

Comment Wall

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

  • No comments yet!
 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service