by Robert spicer
Apr 1, 2021
Can someone please tell me why every cup on the left side of the kiln bloated and cracked on the bottom while every cup on the right side of the kiln was perfectly normal
cone 05 bisque firing using cone 6 stoneware clay
Photos of the fired ware?
Photos of the kiln interior wouldn't hurt either.
Apr 17, 2021
Cancel
Robert spicer
Apr 1, 2021
Norm Stuart
Photos of the fired ware?
Photos of the kiln interior wouldn't hurt either.
Apr 17, 2021