Dry pulling.... - Electric Mid&Hi Fired Ceramics2024-03-29T06:37:42Zhttps://cone6pots.ning.com/forum/topics/dry-pulling?commentId=2103784%3AComment%3A124923&x=1&feed=yes&xn_auth=noI try to throw as thin as pos…tag:cone6pots.ning.com,2015-09-16:2103784:Comment:1249232015-09-16T15:04:44.867ZRobert Coylehttps://cone6pots.ning.com/profile/RobertCoyle
<p>I try to throw as thin as possible. I use a heat gun to stiffen up the last couple of pulls.</p>
<p>I try to throw as thin as possible. I use a heat gun to stiffen up the last couple of pulls.</p> I use a weed burner torch whe…tag:cone6pots.ning.com,2015-09-15:2103784:Comment:1250272015-09-15T05:34:50.704ZGeorge Lewterhttps://cone6pots.ning.com/profile/GeorgeLewter
<p>I use a weed burner torch when my initial shaping gets near to collapse. Have to be careful not to overdo it. 20 - 30 seconds can leave a pot steaming.</p>
<p>I use a weed burner torch when my initial shaping gets near to collapse. Have to be careful not to overdo it. 20 - 30 seconds can leave a pot steaming.</p>