"Clear Base Blue ^6   http://www.wpapotters.blogspot.com/2010/11/cone-6-oxidation-res…"

Norm Stuart replied Apr 16, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"Another typical difference between slow-cooling at 185 F/hr and 50 F/hr with White B…"

Norm Stuart replied Apr 16, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"Another typical difference between slow-cooling at 185 F/hr and 50 F/hr with Jayne S…"

Norm Stuart replied Apr 16, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"Vee's Tenmoku Gold also slow-cooled at 50 degrees F per hour. But EPK is replaced wi…"

Norm Stuart replied Apr 15, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"Vee's Tenmoku Gold - adapted to eliminate the use of Cornwall Stone. More costly at…"

Norm Stuart replied Apr 15, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"107.0%   Ron Roy  Sapphire Blue 37.0%  Frit 3134 26.0%   EPK 17.0%   Silica 16…"

Norm Stuart replied Apr 15, 2013 to Slow Cooling

13 Jun 28, 2017
Reply by Norm Stuart

"Using wood-fired glaze recipes, from John Anthony's Red Hill Pottery site, I discove…"

Norm Stuart replied Apr 15, 2013 to Richard Busch article - Wood fired look from elec kiln

11 Apr 28, 2013
Reply by Norm Stuart

"The Witness Cone 7 was fired with the Cone 6 program - which gives us a perfect Cone…"

Norm Stuart replied Mar 13, 2013 to Witness Cones always indicate one cone hotter than Bartlett Controller V6-CF

4 Mar 13, 2013
Reply by Norm Stuart

"We have a inexperienced people firing the kiln so one reason I bought the Cress E-23…"

Norm Stuart replied Mar 13, 2013 to Witness Cones always indicate one cone hotter than Bartlett Controller V6-CF

4 Mar 13, 2013
Reply by Norm Stuart

"Most of these scales have too many openings to saran-wrap - I tried. It would be nic…"

Norm Stuart replied Mar 6, 2013 to Digital Scales

21 Jul 10, 2014
Reply by Jacob Smith

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2024   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service